Polymer and Process Guides for Polyester Knits
The character of a polyester knit is set long before the knitting machine. Intrinsic viscosity in the reactor, take-up speed on the spinning line, the spinneret cross-section and the dyeing behaviour built into the polymer decide strength, hand, sheen and colour. These seven guides follow that chain from polymer to yarn.
This category brings together the decisions taken upstream of knitting: the PET recipe and its intrinsic viscosity, the speed regime that turns melt into POY, FDY or HOY, the geometry and fineness of each filament, and the polymer modifications that change how the fibre takes colour. Bio-based PET and alternative polyesters such as PTT and PBT belong here as well. Some of these choices, such as the delustrant dose or the colour of a solution-dyed yarn, are fixed when the fibre is born and cannot be changed later. Each value is therefore written into the yarn specification together with the method used to measure it.
The guides are ordered from the polymer towards the yarn. Start with PET chemistry and intrinsic viscosity, then read how melt spinning sets the yarn type. The next two guides deal with the filament itself, its cross-section geometry and its fineness. Cationic-dyeable and solution-dyed polyester follow as two ways of building colour behaviour into the polymer. The guide to bio-based and alternative polyesters completes the category.
Decisions made in this category
| Decision | What to check |
|---|---|
| Which IV should the yarn specification state? | IV in dL/g together with the method and solvent (ASTM D4603 / ISO 1628-5), plus the carboxyl end-group and DEG levels PET Polymer Chemistry: IV, Polycondensation and Why It Matters |
| Does the fabric need POY-based DTY, FDY or HOY? | Take-up speed regime, residual elongation and tenacity in cN/dtex to ISO 2062, with fineness determined to ISO 2060 Melt Spinning and the Formation of POY, FDY and HOY Yarn |
| Which filament cross-section suits the end use? | Trilobal for luster and soil-hiding, multi-channel for wicking, hollow for lightweight warmth; moisture behaviour verified to AATCC 197 and AATCC 195 (MMT) Fibre Cross-Section Engineering: Trilobal, Hollow, Multi-Channel |
| Is a microfilament yarn worth the extra dyehouse effort? | Denier per filament (dpf), controlled dyeing with reductive clearing, fastness to ISO 105-C06 and ISO 105-X12, pilling to ISO 12945-2 Microfilament Science: Micro- and Nano-Denier Yarns |
| How are brilliant shades or two-tone effects achieved? | CDP or ECDP dyed with cationic dyes, dyeing temperature and pressure, and light fastness checked separately to ISO 105-B02 Cationic-Dyeable Polyester (CDP/ECDP) |
| When does solution dyeing make sense? | Volume per colour (MOQ), the narrower palette of heat-stable pigments, approval on a coloured-chip sample and fastness-critical shades such as black, navy and grey Solution-Dyed (Dope-Dyed) Polyester |
| How is a plant-based polyester claim substantiated? | Bio-based carbon content to ASTM D6866, kept apart from any biodegradability claim, which rests on separate standards such as ISO 14855 / EN 13432 Bio-Based and Alternative Polyesters: bio-PET, PTT, PBT |
Key facts
- IV is measured to ASTM D4603 / ISO 1628-5. Apparel-grade PET sits at roughly 0.62–0.68 dL/g, while technical and industrial yarn grades run at ~0.90–1.00+ dL/g. PET Polymer Chemistry: IV, Polycondensation and Why It Matters
- TiO2 added to the melt as a delustrant sets the luster class: below ~0.1% for bright, ~0.3–0.5% for semi-dull and typically ~1.5–2.0% for full-dull fibre. The choice cannot be undone later. PET Polymer Chemistry: IV, Polycondensation and Why It Matters
- POY is spun at ~2,800–3,500 m/min and keeps a residual elongation of typically ~100–160%. FDY, drawn in-line on a spin-draw line, has ~25–40% and is ready to knit without a separate draw step. Melt Spinning and the Formation of POY, FDY and HOY Yarn
- In a hollow fibre the axial void is typically around 5–25% of the cross-sectional area, depending on the application. The trapped still air raises insulation while cutting mass. Fibre Cross-Section Engineering: Trilobal, Hollow, Multi-Channel
- Below 1.0 dpf (roughly 1 dtex) a filament counts as a microfilament. A 1 dtex PET filament is about 10 µm across, against ~70 µm for a human hair. Microfilament Science: Micro- and Nano-Denier Yarns
- High-pressure CDP typically contains about 2.5–4.0 mol% SIPM. ECDP adds a fourth comonomer at roughly 2–8% and can be dyed carrier-free at atmospheric boil (≈100 °C). Cationic-Dyeable Polyester (CDP/ECDP)
- Solution-dyed polyester typically reaches 7–8 on the 1–8 blue wool scale for light fastness (ISO 105-B02) and 4–5 on the 1–5 grey scale for wash fastness (ISO 105-C06). Solution-Dyed (Dope-Dyed) Polyester
- Partly plant-based PET made with bio-MEG typically carries ~30% bio-content, and PTT such as Sorona typically ~37% renewable content. Bio-based content is measured by radiocarbon to ASTM D6866. Bio-Based and Alternative Polyesters: bio-PET, PTT, PBT
Reading order
- PET Polymer Chemistry: IV, Polycondensation and Why It Matters — The hand, strength and drape of a polyester fabric are decided by a single number in the reactor — intrinsic viscosity — long before any yarn exists. IV is measured to ASTM D4603 / ISO 1628-5 and sits at roughly 0.62–0.68 dL/g for apparel-grade PET.
- Melt Spinning and the Formation of POY, FDY and HOY Yarn — A polyester filament’s character is decided not at the knitting machine but in the few-second spinning line where melt turns to solid — and those seconds are governed by take-up speed. The resulting yarn’s linear density is determined to ISO 2060 and its tenacity to ISO 2062.
- Fibre Cross-Section Engineering: Trilobal, Hollow, Multi-Channel — The instant a filament’s cross-section leaves the circle for lobes, grooves and voids, its luster, drying speed and warmth are re-engineered. The effect of cross-section on moisture behaviour is measured to AATCC 195 (MMT) and AATCC 197.
- Microfilament Science: Micro- and Nano-Denier Yarns — Take a filament down to one tenth the thickness of a human hair and you rewrite a fabric’s hand, cover and moisture behaviour — but you pay the bill in the dyehouse and in strength. The cost shows in the dyehouse and at the surface: colour fastness is tracked to ISO 105, pilling to ISO 12945-2.
- Cationic-Dyeable Polyester (CDP/ECDP) — Anionic sulfonate sites grafted onto the polymer chain make ordinary polyester dyeable with cationic (basic) dyes — unlocking brilliant shades and two-tone effects, at the cost of some strength and usually some light fastness. The fastness of the resulting colour is verified with the ISO 105 series.
- Solution-Dyed (Dope-Dyed) Polyester — A coloring method that locks pigment into the fiber while it is still molten, collapsing the water and energy footprint and lifting fastness at its root. The result shows at the top grades of the ISO 105 fastness series.
- Bio-Based and Alternative Polyesters: bio-PET, PTT, PBT — Where plant-derived carbon meets a kinked chain geometry, polyester delivers hand and stretch far beyond fossil PET. Bio-based carbon content is evidenced to ASTM D6866, compostability to EN 13432 / ISO 14855.