Quality and Testing Guides for Polyester Knits
Quality in a polyester knit is decided in two places. In the laboratory, abrasion, pilling, bursting, dimensional change and fastness are measured to named standards. At the inspection table, every roll is scored for visible defects. These four guides explain both gates and how to write them into a specification.
This category brings together the tests a buyer and a mill agree on before production and the checks that decide whether a delivered lot is accepted. A test result only means something together with its method: the same fabric gives different bursting values over different test areas, and different shrinkage percentages under different wash programmes. The guides therefore always state the standard and the conditions next to the number.
The four guides follow the order in which these questions usually come up. Start with the overview of test methods, then read how a lot is approved with the 4-point system, how durability is measured, and where the most common knit defects come from and how they are controlled.
Decisions made in this category
| Decision | What to check |
|---|---|
| Which tests go into the specification? | Abrasion, pilling, bursting, dimensional change and fastness, each with its standard and test conditions Knit Quality Testing: What to Measure in Polyester |
| How is a bursting value written? | The test area (preferably 50 cm² for knits) and the method (hydraulic or pneumatic) together with the kPa value Knit Quality Testing: What to Measure in Polyester |
| Which shrinkage target is acceptable? | The percentage together with the ISO 6330 wash-and-dry programme number Knit Quality Testing: What to Measure in Polyester |
| Is the delivered lot accepted? | Penalty points per 100 square yards under the 4-point system, against the threshold agreed in the contract The 4-Point Inspection System: How a Fabric Lot Gets Approved |
| Which durability test fits the product? | Abrasion for upholstery and bags, pilling for knitwear, bursting and snag for athletic knits Durability Science: Abrasion, Pilling and Snag |
| Why do side seams twist after washing? | Spirality comes from yarn torque, knit structure and stenter heat-setting, and is measured to AATCC 179 / ISO 16322 Knit Defects: Spirality, Barré and Holes — Root Cause and Control |
Key facts
- In the 4-point system a defect up to 3 in (~7.5 cm) scores 1 point and one over 9 in (~23 cm) scores 4. A hole scores 4 points regardless of size. The 4-Point Inspection System: How a Fabric Lot Gets Approved
- No single linear yard can carry more than 4 points, and the total is normalised to 100 square yards. The 4-Point Inspection System: How a Fabric Lot Gets Approved
- A common general-purpose acceptance threshold is around 40 points per 100 yd². Performance and premium work typically asks for ~20–28. The 4-Point Inspection System: How a Fabric Lot Gets Approved
- Pilling is graded 1–5 against reference photographs: 5 means no pilling, 1 means severe pilling. Durability Science: Abrasion, Pilling and Snag
- Light domestic upholstery is typically considered adequate at around 15,000 Martindale rubs. Heavy contract use targets 40,000 and above. Durability Science: Abrasion, Pilling and Snag
- Measured over 7.3 cm² instead of 50 cm², the same fabric gives a higher bursting value, because the smaller area contains fewer weak points. Knit Quality Testing: What to Measure in Polyester
- Spirality is measured to AATCC 179 / ISO 16322. The commercial target is typically ≤5% after washing. Knit Defects: Spirality, Barré and Holes — Root Cause and Control
Reading order
- Knit Quality Testing: What to Measure in Polyester — A knit’s quality shows not in its weight but in the laboratory matrix: abrasion to ISO 12947-2 (Martindale), pilling to ISO 12945-2 (a 1–5 photographic scale), bursting to ISO 13938-1, and dimensional stability to the trio ISO 3759 + ISO 6330 + ISO 5077. In bursting, test area changes the result — 7.3 cm² and 50 cm² give different kPa on the same fabric, which is why the area is always reported.
- The 4-Point Inspection System: How a Fabric Lot Gets Approved — How 4-point fabric inspection works under ASTM D5430 — defects scored 1-4 by size, a cap of 4 points per linear yard, normalised to 100 yd², and common acceptance thresholds — together with the in-house lab gate that completes it (ISO 105 fastness, ISO 3801 weight, ISO 6330/5077 dimensional stability, spectrophotometer ΔE).
- Durability Science: Abrasion, Pilling and Snag — How long a fabric lasts is not a single number: abrasion, pilling, snagging and bursting are independent damage mechanisms, each measured by its own standard method. Each is measured separately: abrasion to ISO 12947-2 (Martindale), pilling to ISO 12945-1/-2.
- Knit Defects: Spirality, Barré and Holes — Root Cause and Control — Knit defects such as spirality, barré, holes/needle lines/drop stitch and slubs are not random; each has a traceable root cause in the yarn, the machine setup or finishing. Positive feed, correct gauge, stenter heat-setting and 4-point inspection are how these defects are prevented or caught. Spirality is measured to AATCC 179 / ISO 16322; defects are scored under the ASTM D5430 four-point system.
Frequently asked questions
How should pilling resistance be written into a specification?
Durability is not a single number. Abrasion, pilling, snagging and bursting are separate damage mechanisms, each measured by its own method. Pilling is measured to ISO 12945-1/-2 and abrasion to ISO 12947-2 (Martindale), and each is written into the specification together with its method.
Are the tests done in your own laboratory?
Basic physical tests are carried out in our own laboratory. Special tests such as UV ageing are carried out by an external laboratory. State the test you need and its method in your request.